Herringboned - Posted - 01/26/2010:  23:55:46


Hi all. I've been lurking here for a while and finally signed up. I'm a longtime regular user of the UMGF, but recently I've realised a lifelong dream, and acquired a National 014. It's all still very new, and I'm real novice when it comes to resonator guitar setup/maintainence. I'm getting there though!

NRP recommend using Flitz or Autosol for cleaning the metal body occasionally (for stubborn marks). I've got some Autosol (couldn't find Flitz in New Zealand). I used it sparingly on a few marks on my guitar - worked great!

I just wonder if I should avoid the sandblasted patterns with the polish? I.e. could I accidentally polish through the sandblasting, or is that impossible?

Sorry if it's a dumb question. I really am a novice!

John in NZ.

meldooby - Posted - 01/27/2010:  07:56:50


You can polish through the nickel plating without much difficulty. I wouldn't
use anything on it but water.

Paul Ryan - Posted - 01/28/2010:  19:26:55


Yeah, I'd use water on that beauty. Even for the cone on my wood body reso, only water. Other than changing strings, I just am really am timid about polishing and cleaning my instruments.

Paul Ryan
ryantunes.com

Terms of Use | Privacy Policy | Privacy Consent (EU/GDPR Only)

Copyright 2026 Reso Hangout. All Rights Reserved.





Hangout Network Help

View All Topics  |  View Categories

0.046875